Tire Natural Reclaimed Rubber

Product Overview

The following is part of the specification data of our general Tire Natural Reclaimed Rubber, we also in the position to produce the goods according to your special request on the quality (like odour, fineness, S/G etc. request). Tensile Strength Elongation at break M.V. ML 100A C@1+4 Water Content Ash Content 12MPA 380% 50-80 1% 10% 10.5MPA 360% 50-80 1% 12% 9MPA 340% 50-80 1.1% 14% 7MPA 280% 50-80 1.1% 16% 6MPA 220% 50-80 1.2% 17%

2025nd Year

Contact Person

No.51 Youyi South Street, Qiaoxi District,

Product Description

The following is part of the specification data of our general Tire Natural Reclaimed Rubber, we also in the position to produce the goods according to your special request on the quality (like odour, fineness, S/G etc. request). Tensile Strength Elongation at break M.V. ML 100A C@1+4 Water Content Ash Content 12MPA 380% 50-80 1% 10% 10.5MPA 360% 50-80 1% 12% 9MPA 340% 50-80 1.1% 14% 7MPA 280% 50-80 1.1% 16% 6MPA 220% 50-80 1.2% 17%