Compressive Strength:
35 Megapascals (MPa )
Weight:
50 Kilograms (kg)
SO3 %:
3.5%
MgO %:
2%
Initial Setting Time:
24 Hours
Color:
Grey
Bending Strength:
40.0 Mpa
Cement Raw Material:
Silicate
Cement Type:
Common Cement
Sand Type:
Manufactured Sand
Sand Fineness:
Fine
Hardening Feature:
Rapid Hardening
Heat of Hydration:
Low Heat
Feature:
Corrosion Resistance
Contact Person
Plot No. A32, 2 Nd, Near by Todkar Township, Sasanenagar, Hadapsar,
This is a 50-kilogram rapid hardening low heat corrosion resistance fine cement that is used to build roads and railways. It is made from silicate, common cement, manufactured sand, and fine sand. The cement is used to build roads and railways with a compressive strength of 35 MPa. The initial setting time is 24 hours, the SO3 % is 3.5%, the MgO % is 2%, and the color is grey.
Compressive Strength: | 35 Megapascals (MPa ) |
Weight: | 50 Kilograms (kg) |
SO3 %: | 3.5% |
MgO %: | 2% |
Initial Setting Time: | 24 Hours |
Color: | Grey |
Bending Strength: | 40.0 Mpa |
Cement Raw Material: | Silicate |
Cement Type: | Common Cement |
Sand Type: | Manufactured Sand |
Sand Fineness: | Fine |
Hardening Feature: | Rapid Hardening |
Heat of Hydration: | Low Heat |
Feature: | Corrosion Resistance |